What are the process conditions that affect the damage of the induction furnace lining
During the use of the intermediate frequency furnace , the thickness of the refractory used for the furnace lining is only 70-110mm. The inner side is in contact with the high-temperature molten metal, and the outer side is close to the water-cooled coil. The temperature difference between the inner and outer sides of the refractory is large. Under the conditions of use in aggressive environments. The main process conditions that affect the damage of the furnace lining include: smelting temperature, degassing time, one-time degassing amount, chemical composition of slag and steel (iron) type produced. The main influencing factors that damage the furnace lining are: chemical corrosion of slag, flaking of refractory structure and thermal corrosion. As the furnace capacity increases, the proportion of heat lost from the surface of the molten steel decreases. The slag temperature is higher than that of a small-capacity furnace, and the fluidi...